Features:
¡ñThe best temperature characteristics in the rare-earth magnet family
¡ñManufactured by powder metallurgical process involving the sintering of powder under vacuum.
¡ñBoth grades of SmCo5 and Sm2Co17, commonly referred to as 1:5 and 2:17 material are available.
¡ñGood corrosion resistance and no special surface treatment required excellent for compact designs
¡ñUsed in where high working temperature is a major concern.
¡ñGrinding and slicing operations possible
Applications:
Applied to various electric motors, instruments, sensors, detectors, radar, and other high-tech equipment.
Specifications:
Grade
|
Br
|
HcB
|
HcJ
|
(BH)max
|
Tc
|
Tw
|
¦Á£¨Br£©
|
¦Á£¨Hcj£©
|
T
|
T
|
kA/m
|
kA/m
|
kJ/m3
|
¡æ
|
¡æ
|
%/¡æ
|
%/¡æ
|
KGs
|
KGs
|
KOe
|
KOe
|
MGOe
|
RECo5 119/127
|
0.83
|
0.81
|
620
|
1274
|
127
|
119
|
750
|
250
|
-0.04
|
-0.3
|
8.3
|
8.1
|
7.8
|
16
|
16
|
15
|
RECo5 135/127
|
0.87
|
0.84
|
645
|
1274
|
143
|
135
|
750
|
250
|
-0.04
|
-0.3
|
8.7
|
8.4
|
8.1
|
16
|
18
|
17
|
RECo5 151/127
|
0.92
|
0.89
|
680
|
1274
|
159
|
151
|
750
|
250
|
-0.04
|
-0.3
|
9.2
|
8.9
|
8.5
|
16
|
20
|
19
|
RECo5 159/127
|
0.95
|
0.93
|
710
|
1274
|
167
|
159
|
750
|
250
|
-0.04
|
-0.3
|
9.5
|
9.3
|
8.9
|
16
|
21
|
20
|
RECo5 175/119
|
0.98
|
0.96
|
730
|
1194
|
183
|
175
|
750
|
250
|
-0.04
|
-0.3
|
9.8
|
9.6
|
9.2
|
15
|
23
|
22
|
RE(Sm)Co5 151/104
|
0.92
|
0.89
|
680
|
1035
|
159
|
151
|
750
|
250
|
-0.04
|
-0.3
|
9.2
|
8.9
|
8.5
|
13
|
20
|
19
|
RE(Sm)Co5 159/104
|
0.95
|
0.93
|
710
|
1035
|
167
|
159
|
750
|
250
|
-0.04
|
-0.3
|
9.5
|
9.3
|
8.9
|
13
|
21
|
20
|
RE(Sm)Co5 151/159
|
0.92
|
0.89
|
680
|
1592
|
159
|
151
|
750
|
250
|
-0.04
|
-0.3
|
9.2
|
8.9
|
8.5
|
20
|
20
|
19
|
RE(Sm)Co5 159/159
|
0.95
|
0.93
|
710
|
1592
|
167
|
159
|
750
|
250
|
-0.04
|
-0.3
|
9.5
|
9.3
|
8.9
|
20
|
21
|
20
|
RE(Sm)Co5 175/119
|
0.98
|
0.96
|
730
|
1194
|
183
|
175
|
750
|
250
|
-0.04
|
-0.3
|
9.8
|
9.6
|
9.2
|
15
|
23
|
22
|